Air-SAGD technology for super-heavy oil reservoirs
Yongrong GAO,Erpeng GUO,Dehuang SHEN,Bojun WANG
Table 1 Viscosity test data before and after air oxidation of super-heavy oil sample.
No. Temperature/°C Viscosity/(mPa?s)
Unoxidized dead oil 150 °C, 12.0 cm3/g 200 °C, 12.0 cm3/g 250 °C, 2.5 cm3/g 250 °C, 6.0 cm3/g 250 °C, 12.0 cm3/g
1 50 135 800.0 392 500.0 8 401 000.0 322 500.0 601 600.0 9 906 700.0
2 60 68 500.0 98 240.0 2 171 000.0 88 780.0 178 500.0 3 988 400.0
3 70 25 710.0 35 000.0 477 100.0 29 760.0 56 080.0 2 251 800.0
4 80 14 850.0 15 700.0 135 400.0 17 190.0 26 400.0 583 800.0
5 90 6 980.0 8 970.0 59 800.0 8 080.0 11 200.0 199 330.0
6 100 4 120.0 5 010.0 24 980.0 4 770.0 6 500.0 62 270.0
7 120 1 408.0 1 820.0 6 240.0 1 630.0 2 150.0 10 700.0
8 160 292.3 361.2 887.5 340.8 446.3 1 090.0
9 180 170.4 207.2 425.6 198.7 260.2 440.8
10 200 90.6 115.6 208.8 105.6 138.4 235.6
11 220 57.3 71.5 119.1 66.8 87.5 120.3
12 250 33.5 38.5 57.5 39.1 51.2 63.7